Some marbles exhibit hysteretic behavior after repeated heating and cooling cycles. This hysteresis is typically evident by a bowing of the marble panels, and can normally be eliminated if the panels are of sufficient thickness. Research of the particular marble should be done to determine its vulnerability to this phenomenon.